DeAI Research
Source · Gōsei jushi

Comparison of Heating Behavior of Expandable Styrene Polymers Containing Graphite and Normal Expandable Styrene Polymers

2012Li Yueming

cid 80734400c1851ec7d7e1dbbee1c512013ce5f6a8d7b991d88ab316595467f86f · original · via openalex

Title: Comparison of Heating Behavior of Expandable Styrene Polymers Containing Graphite and Normal Expandable Styrene Polymers
Authors: Li Yueming
Venue: Gōsei jushi
Year: 2012
Canonical: openalex:https://openalex.org/W2370441666
URL: https://openalex.org/W2370441666
Collector: openalex
OA: false

ABSTRACT
The mass loss and pyrolytic deformation of graphite-embedded polystyrene(GEPS) and normal expandable polystyrene(EPS) foams were investigated by thermogravity analyzer and stereo pyroscope.As seen from the thermogravity curves,both EPS and GEPS foams presented two obvious stages of mass loss,and the high-temperature stage gave the main contribution of the total mass loss.Besides,it was found that the pyrolytic point θi2 of GEPS reached to 382 ℃,significantly higher than that of EPS(236.0 ℃).Meanwhile,the maximan pyrolytic rate θmax2 reached to 415.2 ℃,also obviously exceeded over that of EPS(263.7 ℃).The pyroscope observation revealed that GEPS foams showed off the deformation at 128 ℃ while began to melt with fluxibily at 260 ℃,much higher over EPS foams.